N
|
Element
|
Ga 7N |
Ga 6N
|
Ga 4N
|
ppb wt
|
ppb wt
|
ppm wt
|
1
|
Li
|
<0.1
|
<0.5
|
|
2
|
Be
|
<0.1
|
<0.6
|
|
3
|
B
|
<0.5
|
<2
|
|
4
|
F
|
<4
|
|
|
5
|
Na
|
<0.5
|
<4
|
|
6
|
Mg
|
<0.5
|
<4
|
|
7
|
Al
|
<1
|
<4
|
<1
|
8
|
Si
|
<5
|
<20
|
<2
|
9
|
P
|
<1
|
<10
|
|
10
|
S
|
<2
|
<10
|
|
11
|
Cl
|
<5
|
<20
|
|
12
|
K
|
<4
|
<6
|
|
13
|
Ca
|
<5
|
<12
|
|
14
|
Sc
|
<0.03
|
<0.6
|
|
15
|
Ti
|
<0.1
|
<1.5
|
<1
|
16
|
V
|
<0.03
|
<1.5
|
|
17
|
Cr
|
<1
|
<2
|
<2
|
18
|
Mn
|
<0.5
|
<1.5
|
<1
|
19
|
Fe
|
<2
|
<4
|
<10
|
20
|
Co
|
<0.05
|
<0.8
|
|
21
|
Ni
|
<1
|
<4
|
<5
|
22
|
Cu
|
<2
|
<4
|
<5
|
23
|
Zn
|
<1
|
<4
|
<5
|
24
|
Ge
|
<10
|
<30
|
<0.05
|
25
|
As
|
<0.5
|
<2
|
<1
|
26
|
Se
|
<6
|
<6
|
|
27
|
Br
|
<5
|
|
|
28
|
Rb
|
<0.3
|
|
|
29
|
Sr
|
<2
|
<2
|
|
30
|
Y
|
<0.5
|
|
|
31
|
Zr
|
<0.6
|
<2
|
|
32
|
Mo
|
<0.5
|
<2
|
|
33
|
Ag
|
<40
|
<50
|
|
34
|
Cd
|
<4
|
<10
|
<5
|
35
|
In
|
<1
|
<5
|
<20
|
36
|
Sn
|
<8
|
<10
|
<20
|
37
|
Sb
|
<0.6
|
<2
|
<2
|
38
|
Te
|
<0.8
|
<2
|
<1
|
39
|
Ba
|
<1
|
<5
|
|
40
|
La
|
<0.2
|
<1
|
|
41
|
W
|
<0.3
|
<2
|
|
42
|
Pt
|
<1
|
<2
|
|
43
|
Au
|
<5
|
<5
|
<0.5
|
44
|
Hg
|
<5
|
<10
|
<5
|
45
|
Tl
|
<0.1
|
<1
|
|
46
|
Pb
|
<0.3
|
<3
|
<20
|
47
|
Bi
|
<0.5
|
<3
|
<10
|
48
|
Th
|
<0.03
|
<0.5
|
|
49
|
U
|
<0.03
|
<0.5
|
|
|

|
|

|
|
- recycling of GaAs, GaP and other Ga related scraps (contaminated with water, oil, boron oxide,
pBN, epoxy, cement, alumina, etc.) with min Ga content 5 %

- our own proprietary technology is waste free

- refining of Gallium to 4N (99,99 %), 6N (99,9999 %) or 7N (99,99999 %)

- a unique technology for removing Germanium from Gallium down to 10 ppb wt

- typical yield from GaAs to Ga process is 97 % and 99 % from refining Ga 4N to 6N or 7N

- short turnaround is platitude

- each lot is analysed for purity by GDMS and a certificate is enclosed

- packaging according to IATA regulations in certified boxes and PE bottles filled under pure nitrogen

|